20YJ-134 < 20200122111920-386239 > pub
  • technique: XRF
  • device: XRF Rigaku RIX300
  • modified at 2020-01-22
  • stone: 20YJ-134
measured value uncertainty unit description
[SiO2] 61.84 %
[TiO2] 0.74 %
[Al2O3] 14.79 %
[MnO] 0.04 %
[CaO] 6.18 %
[MgO] 3.57 %
[Na2O] 3.68 %
[K2O] 2.01 %
[P2O5] 0.32 %
[LOI] 3.39 %
total 99.89 %
[Mg#] 68.2
[Fe2O3T] 3.33 %
name global-id
name spots global-id